DictionaryForumContacts

 G.O.A.N.

link 17.01.2008 4:31 
Subject: сварка: mill tempering temperature
контекст:
Note that it has been confirmed that for the three heats where weld through thickness hardness is between 251 and 255HV (heats ####, ###, ####), this PWHT temperature is less than the mill tempering temperature.

 Mrs

link 17.01.2008 6:27 
имхо:
...для трех плавок твердость по толщине сварного шва такая-то
...менее температуры отпуска (проката)

 